Glass flexible / plastic stringers

Tests of different formulations.

PVA melting. Did not work. PVA became soft, but started burning without becoming liquid.

PVA water soluble film. Add 15 g film (~ two layers), add water to dissolve (around 100 ml, did not measure), stirred 5 min, it nearly all went into solution, viscosity was low. Add 15 g glass powder, heat on hot plate at 60C until water evaporated.

PLA dissolved in DCM (dichloromethane). Added 15 g PLA pellets to DCM, ~100-150 ml.

Higher mol weight PVA + CMC.
ABS in acetone


Liquid Glass Line / Flexi-Glass, Liquid Stringer products, instructions.
Flexi-Glass composition from MSDS ,link:
< 2% CMC (carboxy methyl cellulose)
< 2% phosphated polyester (unknown)
-aid adhesion, may raise combustion temp
9 – 12% PVA (polyvinyl alcohol)
< 2% diethylene glycol butyl ether (2-(2-butoxyethoxy)ethanol) (solvent)
< 2% ethanol
< 2% surfactant (unknown)
< 2% tripropylene glycol ether (guess)
-solvent
Instructions: 1 part 70% isopropyl alcohol : 1 1/2 parts Glass Color Powder : 1 part Flexi-Glass Medium
The transfer sheet is likely PET (polyethelene terephthalate).
Lines can be ~3 mm.

Liquid Stringer composition from MSDS link, instructions
< 2% CMC (carboxy methyl cellulose)
< 2% phosphated polyester (unknown)
-aid adhesion, may raise combustion temp
< 16% diethylene glycol butyl ether (2-(2-butoxyethoxy)ethanol) (solvent)
< 2% ethanol
< 2% surfactant (unknown)
< 2% tripropylene glycol ether (guess)
-solvent
Lines are ~4-6 mm wide.